S30403, Wrought Austenitic Stainless Steels, Steel (state: None)

Material type: Wrought Austenitic Stainless Steels

Exergy values

Method Minimum / kJ/kg Mean / kJ/kg Maximum / kJ/kg
substance_composition 7174.6 7454.6 7612.6

Composition

Molecular Mass: 54.84 / g/mol

Substance Mass Fraction
Cr 0.1900
C 0.0003
Mn 0.0200
Si 0.0100
Fe 0.6797
Ni 0.1000
Reference: (Perry & Green, 1997)

Proximate analysis

No proximate analysis data.

Ultimate analysis

No ultimate analysis data.

Heating values