Material type: Terylene
Method | Minimum / kJ/kg | Mean / kJ/kg | Maximum / kJ/kg |
---|---|---|---|
heating values: Huang et al (2016) HHV | 22625.9 | 22625.9 | 22625.9 |
heating values: Song et al (2012) HHV | 21948.3 | 21948.3 | 21948.3 |
heating values: Zhang et al (2016) HHV | 22144.0 | 22144.0 | 22144.0 |
ultimate: Hongliang et al (2017) | 22793.5 | 22793.5 | 22793.5 |
ultimate: Shieh & Fan (1982) | 22653.1 | 22653.1 | 22653.1 |
ultimate: Song et al (2012) | 24113.9 | 24113.9 | 24113.9 |
ultimate: Stepanov (1995) | 21843.8 | 21843.8 | 21843.8 |
No substance composition data.
Component | Wt % |
---|---|
VM | 88.60 |
FC | 10.91 |
A | 0.49 |
Reference: (Eboh, et al., 2016)
Component | Wt % |
---|---|
Ash | 0.49 |
C | 61.86 |
O | 32.96 |
H | 4.12 |
N | 0.29 |
S | 0.28 |
Cl | 0.00 |
Reference: (Eboh, et al., 2016)
Heating value | kJ/kg |
---|---|
HHV | 20963.0 |
LHV | None |
Reference: (Eboh, et al., 2016)